Local stress state of pipelines with misalignment connections

Authors

  • Z. S. Yaskovets IPMits named after GS Pisarenko of the National Academy of Sciences of Ukraine, Kiev, Ukraine https://orcid.org/0000-0001-7629-8868
  • І. P. Seliverstova IPMits named after GS Pisarenko of the National Academy of Sciences of Ukraine, Kiev, Ukraine
  • М. V. Borodii IPMits named after GS Pisarenko of the National Academy of Sciences of Ukraine, Kiev, Ukraine

DOI:

https://doi.org/10.20535/2521-1943.2019.85.132114

Keywords:

axial misalignment, difference-weld joints, concentration of stresses

Abstract

The relevance of the development of analytical methods for the determination of the stressed state of pipelines with differently-thickened compounds is noted. On the basis of shell solutions, an analytical method for determining the basic force and deformation parameters for analyzing the stressed state of pipes with imperfections of transverse welds in the form of axial misalignment is obtained, which simulates common defects in the shape of pipe welding-edge misalignment and thickness change. The numerical simulation for checking the results of analytical analysis showed high convergence of the results in stress concentration zones.

Author Biographies

Z. S. Yaskovets, IPMits named after GS Pisarenko of the National Academy of Sciences of Ukraine, Kiev

Аспірантка

І. P. Seliverstova, IPMits named after GS Pisarenko of the National Academy of Sciences of Ukraine, Kiev

Аспірантка

References

  1. DSTU-N B V.2.3-21:2008
  2. API 579-1/ASME FFS-1, 2016.
  3. Ghaednia, H. and Das, S. (2017), “Structural Performance of Oil and Gas Pipe with Dent Defect”, Journal of Pipeline Systems Engineering and Practice, July 13, vol.9, no. 1, https://doi.org/10.1061/(ASCE)PS.1949-1204.0000301
  4. Ying Wu, Na Tang, and Peng Zhang, (2015), “The Comparison of Dented Pipeline Displacement Calculation Methods”, Engineering Failure Analysis, November, vol. 57, pp. 562-573.
  5. Orynyak, I.V., Bogdan, A.V. and Rozgonyuk, V.V. (2004), “Ductile fracture model for a pipe with a dent”, Ed. R. Denys (Ostend, Belgium), Proc. 4th Int. Conf. on Pipeline Technology, vol. 5, pp. 949-960.
  6. Andronov, I.N., Gavryushin, S.S. and Zakharenkov, D.V.(2011), “Analiz vliyaniya defektov v zone svarnogo shva na prochnost' truboprovoda”, Izvestiya vysshikh uchebnykh zavedenii, Mashinostroenie, Moskovskii gosudarstvennyi tekhnicheskii universitet im. N.E. Baumana, рр. 5-10.
  7. Gol'dshtein, A.E. and Yakimov, E.V.(2010), “Izmerenie otkloneniya ot soosnosti svarnykh soedinenii buril'nykh trub”, Polzunovskii vestnik, no. 2, pp. 65-68.
  8. Chaudhari, S.B. and Belkar, S.B. (2014), “Experimental and Analytical Investigation in Circumferential Joint”, International Journal of Mechanical Engineering and Information Technology, IJMEIT, vol. 2, no. 6, pp. 453-465.
  9. Ahmed, W.K. and Mourad, A-H. I. (2013), “Strengthening of Misaligned Welded Pipes with Outer Circumferentially Crack Using FRP Bandage Finite Element Analysis”, Journal of Mechanical Engineering and Technology, Sept., vol. 1, no. 2, pp. 66-73, DOI: 10.18005/JMET0102005
  10. Orynyak, I., Bogdan, A. and Selivestrova, I. (2016),The Application of Long and Short Cylindrical Shell Solutions for Stress and Flexibility Determination in a Single Mitred Bend, Proceedings of the ASME 2016 Pressure Vessels and Piping Conference PVP2016-63598, July 17-21, Vancouver, p. 10.

Published

2019-04-14

How to Cite

[1]
Z. S. Yaskovets, Seliverstova І. P., and Borodii М. V., “Local stress state of pipelines with misalignment connections”, Mech. Adv. Technol., no. 1(85), pp. 35–40, Apr. 2019.